Poly(3-butoxypropylene oxide)
CROW logo
Poly(3-butoxypropylene oxide)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyglycol
COMMON NAMESPoly(3-butoxypropylene oxide)
STRUCTURE BASED NAME Poly(2-(butoxymethyl)oxirane), Poly[oxy(1-(butoxymethyl)ethylene)]
ACRONYMS  
CAS #  
CurlySMILES O{-}C(COCCCC)C{n+}
 

IDENTIFIERS OF MONOMER(S)

CAS # 2426-08-6
COMMON NAMES 2-(Butoxymethyl)oxirane, n-Butyl glycidyl ether
SMILES CCCCOCC1CO1
Std. InChI InChI=1S/C7H14O2/c1-2-3-4-8-5-7-6-9-7/h7H,2-6H2,1H3
Std. InChIKey YSUQLAYJZDEMOT-UHFFFAOYSA-N
STRUCTURE
(2-(Butoxymethyl)oxirane
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume Vm mL mol-1 133
Density ρg mL-1 0.98 
Solubility Parameter δMPa1/2   
Molar Cohesive Energy EcohJ mol-1   
Glass Transition Temperature TgK 194 
Molar Heat Capacity CpJ (mol K)-1   
Entanglement Molecular Weight Meg mol-1   
Index of Refraction nnone 1.47  
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 130.19
Van-der-Waals Volume VvWmL mol-1 75.9
Molar Volume VmmL mol-1 122 - 135129
Density ρg mL-1 0.96 - 1.071.01
Solubility Parameter δMPa1/2 17.6 - 18.818.0
Molar Cohesive Energy EcohJ mol-1 40900 - 4320041900
Glass Transition Temperature Tg K 191 - 210 201
Molar Heat Capacity CpJ (mol K)-1 265 - 281274
Entanglement Molecular Weight Meg mol-1   
Index of Refraction nnone 1.46 - 1.471.47

  Last updated: August 13, 2016